Prestressing wires — stress-relaxation and stress-corrosion up to date

$15.00

The characteristics of wire used in prestressing of concrete are described, and the free loop test for determining stress corrosion of such wire is discussed. The effects of oil tempering, cold drawing, electroplating, and carbon content on stress corrosion are presented. Stress relaxation and fatigue are also considered.

Description

The characteristics of wire used in prestressing of concrete are described, and the free loop test for determining stress corrosion of such wire is discussed. The effects of oil tempering, cold drawing, electroplating, and carbon content on stress corrosion are presented. Stress relaxation and fatigue are also considered.

Additional information

Author(s)

Spare, G.T.U.S. Steel Corp.

Publication/Event/Pages

Wire & Wire Products29(12): 1421-1424, 1492-1493 1954, Paper presented at WAI 24th Annual Convention, Detroit, MI USA

Year

1954